Alloy |
Approx. Pouring Temp. |
Density |
Characteristics |
|
BP |
350 oC |
7.3 g/cm3 |
Non toxic, Strong, takes a high polish |
|
92 |
300 oC |
7.3 g/cm3 |
Lead free, strong, good detail |
|
KP |
280 oC |
7.6 g/cm3 |
Softer than 92, good detail, low pouring temp |
|
C |
300 oC |
9.3 g/cm3 |
Soft alloy, good detail |
|
29 |
320 oC |
10.0 g/cm3 |
- |
|
20 |
340 oC |
10.2 g/cm3 |
- |
|
18 SOLDER |
145 oC |
- |
Good fluidity, good wetting |
|
HAYESOL
70 |
68 oC |
- |
Low melting point alloy for fire sprinklers, pipe bending and proof pattern making |
|
HAYESOL
11 |
425 oC |
- |
High load tin base bearing alloy |
|
HAYESOL
11 |
480 oC |
- |
Same as above but with higher fatigue resistance |
|
HAYESOL
12 |
400 oC |
- |
High strength hard tin base bearing alloy |
|
HAYESOL
13 |
370 oC |
- |
Cost effective lead base bearing alloy |
|
HAYESOL 100 |
100 oC |
- |
Cadmium free fusible alloy for X-Ray shielding |
|
UWBA |
400 oC |
- |
For stern bearings. Alloy is equipotential to iron |
|
Antimonial Lead |
- |
- |
Used for boat keels |